SURFACE SPALLING OR DETERIORATION
REPAIR PROCEDURES
After cuts are made, deepen the defect to the
depth shown with a bush hammer or other means.
2. Mix Armor-Hard or MM-80 epoxy. Add aggregate to liquid epoxy. Mix per instructions and apply. Compact mortar with trowel from kit to ensure full contact. Trowel smooth or broom finish during epoxy cure non-skid texture.
OPTION: Spal-Pro 2000 Polyurea Repair Polymer can be used if access time is critical. | |||||||||